MagneticPhase Epoxy gallium_nitride Aluminium_Oxide Potential norganic solar_cell Hair Photovoltaics CalciumHydroxyapatite Calcite Anneal Crystal Beads HexacontaneFilm hard_disk Flake MagneticArray Optoelectonics FrictionalForceMicroscopy HighAcpectRatio SiWafer lithography BloodCell small_scan CeramicCapacitor Thermal Etch CHRYSALIS_INC OpticalWaveguides molecular_beam MultiLayerCeramicCapacitor ForceDistanceSpectroscopy Ceramic FAPbI3
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ExFoliated graphene on SiO₂/Si wafer
Scanning Conditions
- System : FX40
- Scan Mode: Non-Contact, Lithography
- Scan Rate : 1 Hz
- Scan Size : 10μm×10μm
- Pixel Size : 256×256
- Cantilever : PPP-EFM (k=2.8N/m, f=75kHz)
- Litho. Condition : Force 200nN, Writing speed 0.2 μm/s , AC bias 10 V @ 40 kHz, Humidity ~90% RH