Edwin KAIST medical semifluorinated_alkanes ImideMonomer CrossSection Zhi Tin disulfide PtfeFilter Regensburg Collagen FrictionForce Yeditepe margarine Indium_tin_oxide I-VSpectroscopy SurfaceChange norganic frequency_modulation NiFe Ito MolybdenumDisulfide UTEM 2dMaterials PetruPoni Logo Chrome self_healing BariumTitanate Piezoresponse CNT STO Molybdenum Forevision Gallium_Arsenide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ER 316L Stainless Steel
The ferrite MFM phase has a striped appearance due to its ferromagnetic behavior, while the paramagnetic austenite phase shows a uniform appearance.
Scanning Conditions
- System: NX20
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm